Physical Properties Metric English Comments
Vapor Pressure 2.10e-8 - 0.0100 bar
0.0000158 - 7.50 torr
Average value: 0.00250 bar Grade Count:4
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..