Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00533 bar @Temperature 20.0 °C |
4.00 torr @Temperature 68.0 °F |
Vapor density: 4.4 |
LG Chemical Butyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Vapor Pressure | 0.00533 bar @Temperature 20.0 °C |
4.00 torr @Temperature 68.0 °F |
Vapor density: 2.5 |
LG Chemical 2-Ethyl Hexyl Acrylate Features: Low Color- Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity -Through the multistage .. |
|||
Vapor Pressure | 0.00533 bar @Temperature 20.0 °C |
4.00 torr @Temperature 68.0 °F |
ExxonMobil Method |
ExxonMobil Exxsol™ D30 Dearomatized Fluid Availability: Africa & Middle East, Europe, Asia Pacific and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Vapor Pressure | 0.00533 bar @Temperature 20.0 °C |
4.00 torr @Temperature 68.0 °F |
ExxonMobil Method |
ExxonMobil Exxsol™ DSP145/160 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Vapor Pressure | 0.00533 bar @Temperature 20.0 °C |
4.00 torr @Temperature 68.0 °F |
ExxonMobil Method |
ExxonMobil Varsol™ 30 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |