Polymer Property : Vapor Pressure = 0.0203 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0203 bar

@Temperature 200 °C
15.2 torr

@Temperature 392 °F
PolyOne Synplast™ 901P-N Di (Nonyl, Decyl, Undecyl) Phthalate
Linear phthalate esterInformation provided by PolyOne
Vapor Pressure 0.0203 bar

@Temperature 200 °C
15.2 torr

@Temperature 392 °F
PolyOne Synplast™ DUP-E Di Undecyl Phthalate
Linear C11 phthalate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Vapor Pressure 0.0203 bar

@Temperature 200 °C
15.2 torr

@Temperature 392 °F
PolyOne Synplast™ 901P-E Di (Nonyl, Decyl, Undecyl) Phthalate
Linear phthalate esterNote: Contains 0.1 - 0.15 wt% 1,1,3-Tris (2-methyl-4-hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne