Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.173 bar @Temperature 25.0 °C |
130 torr @Temperature 77.0 °F |
|
Enviro Tech International EnSolv® Ionic n-Propyl Bromide Vapor Degreasing Solvent EnSolv-Ionic is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane, HCFC-141b, Freon and other hazardous or discontinued vapor degreasing, ultrasonic and manual cleanin.. |