Vapor Pressure <= 0.000533 bar

@Temperature 20.0 °C
<= 0.400 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Exxsol™ D60 Dearomatized Fluid
Availability: Africa & Middle East, Asia Pacific, Europe, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil
Vapor Pressure 0.000533 bar

@Temperature 20.0 °C
0.400 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Isopar™ K Naphtha Isoparaffin Fluid
Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation pr..
Vapor Pressure 0.000533 bar

@Temperature 20.0 °C
0.400 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Varsol™ 60 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil