Polymer Property : Vapor Pressure = 1.108 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 1.108 bar

@Temperature 37.8 °C
831.1 torr

@Temperature 100 °F
Saturated
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)
PPVE is a colorless transparent liquid and important monomer of organic fluoride material, which can also be used to introduce fluoride functional groups.Main Applications:PPVE is fluoride vinyl eth..