Polymer Property : Vapor Pressure = 13.71 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 13.71 bar

@Temperature 25.0 °C
10280 torr

@Temperature 77.0 °F
Shandong Dongyue Polymer HFC-125 Pentafluoroethane Refrigerant, CHF2CF3