Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00375 bar @Temperature 20.0 °C |
2.81 torr @Temperature 68.0 °F |
|
LyondellBasell PTB Propylene glycol tertiary butyl ether Information provided by Lyondell. |