Vapor Pressure 0.0413 bar

@Temperature 20.0 °C
31.0 torr

@Temperature 68.0 °F
LyondellBasell TBAcâ„¢ Solvent, Tertiary butyl acetate
Information provided by Lyondell.
Vapor Pressure 0.0413 bar

@Temperature 20.0 °C
31.0 torr

@Temperature 68.0 °F
LyondellBasell TEBOL® 99 High Purity TBA, Tertiary butyl alcohol
Information provided by Lyondell.