Polymer Property : Vapor Pressure = 76.0 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.101 bar

@Temperature 20.0 °C
76.0 torr

@Temperature 68.0 °F
Indium Corp. Germanium Corporation® GeCl4 Germanium Tetrachloride
Germanium tetrachloride is a colorless liquid. It is used as an intermediate in the production of purified germanium dioxide and germanium metal, but more predominantly used as a reagent in fiber o..