Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 4.06 cm

@Temperature 280 °C
1.60 in

@Temperature 536 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers..
Neck In 4.06 cm

@Temperature 315 °C
1.60 in

@Temperature 599 °F
164 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 251 Low Density Polyethylene Resin (European Grade)
Product Description: LD 251 is an LDPE extrusion coating grade, offering:low neck-in excellent heat sealablity (ie high seal speeds and/or seal temperatures mostly required in high speed form-fill a..
Neck In 4.06 cm

@Temperature 315 °C
1.60 in

@Temperature 599 °F
492 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade)
Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:Low volatiles..