Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 11.7 cm @Temperature 295 °C |
4.61 in @Temperature 563 °F |
328 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and .. |