Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 5.59 cm @Temperature 295 °C |
2.20 in @Temperature 563 °F |
656 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyet.. |