Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.000800 g/m²/day @Temperature 38.0 °C |
0.0000515 g/100 in²/day @Temperature 100 °F |
90% RH; ISO 15106-3 |
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and.. |