Polymer Property : Water Vapor Transmission = 0.00322 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.0500 g/m²/day
0.00322 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell..
Water Vapor Transmission 0.0500 g/m²/day
0.00322 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..