Water Vapor Transmission 0.0600 g/m²/day
0.00386 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.