Physical Properties Metric English Comments
Water Vapor Transmission 0.09312 - 18.624 g/m²/day

@Temperature 37.8 - 38.0 °C
0.005997 - 1.1994 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 5.22 g/m²/day Grade Count:113
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..