Polymer Property : Water Vapor Transmission = 0.0161 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.0000250 - 0.250 g/m²/day
0.00000161 - 0.0161 g/100 in²/day
Average value: 0.111 g/m²/day Grade Count:8
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..