Polymer Property : Water Vapor Transmission = 0.0170 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.264 g/m²/day
0.0170 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..