Polymer Property : Water Vapor Transmission = 0.0419 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.650 g/m²/day
0.0419 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Dow Saran® 560 Clear Plastic Barrier Film
Saran™ 560 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 6 gauge.Information provided by Dow