Physical Properties Metric English Comments
Water Vapor Transmission 0.780 g/m²/day
0.0502 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film  (discontinued **)
Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell.
Water Vapor Transmission 0.780 g/m²/day
0.0502 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film  (discontinued **)
Description: ACLAR® Cx™ 8A is a heat sealable coextruded CTFE film.Information provided by Honeywell.