Physical Properties Metric English Comments
Water Vapor Transmission 0.0620 g/m²/day
0.00399 g/100 in²/day
86°F (30°C) / 60%RH; ASTM F1249
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film
Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf..
Water Vapor Transmission 0.0620 g/m²/day
0.00399 g/100 in²/day
104°F (40°C) / 75%RH; ASTM F1249
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..