Physical Properties Metric English Comments
Water Vapor Transmission 2.02 g/m²/day

@Temperature 38.0 °C
0.130 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Metallyte™ 38MW280 OPP Film
Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability..