Water Vapor Transmission 9.30 - 9.30 g/m²/day

@Temperature 38.0 - 38.0 °C
0.599 - 0.599 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 9.30 g/m²/day Grade Count:1