Physical Properties Metric English Comments
Water Vapor Transmission 16.7 g/m²/day
1.08 g/100 in²/day
1 atm, 38°C, 100% RH; ASTM D1249
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..