Polymer Property : Water Vapor Transmission = 1.20 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 15.5 - 18.6 g/m²/day
0.998 - 1.20 g/100 in²/day
Average value: 17.4 g/m²/day Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..