Water Vapor Transmission 116 g/m²/day
7.47 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat..