Physical Properties Metric English Comments
Water Vapor Transmission 181 g/m²/day
11.7 g/100 in²/day
100°F (37.8°C) / 97%RH; ASTM F1249
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 1.0 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..