Physical Properties Metric English Comments
Water Vapor Transmission 145 - 295 g/m²/day
9.34 - 19.0 g/100 in²/day
Average value: 220 g/m²/day Grade Count:4
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..