Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 14.3 - 217 g/m²/day | 0.920 - 14.0 g/100 in²/day | Average value: 126 g/m²/day Grade Count:3 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |