Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 48.0 g/m²/day | 3.09 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |