Polymer Property : Water Vapor Transmission = 3.30 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 3.30 g/m²/day
0.213 g/100 in²/day
ASTM F372
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Grade
PETROTHENE LP510300 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. LP510300 is recommended ..
Water Vapor Transmission 3.30 g/m²/day
0.213 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 170 ASB-X OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as..