Water Vapor Transmission 62.1 g/m²/day
4.00 g/100 in²/day
at 1 atm; ASTM E96
Dow INTEGRAL™ 933 Tough Film for Lamination to Porous Substrates
INTEGRAL 933 Adhesive Film has a low melting, high flow adhesive layer that is useful for bonding to substrates such as polyurethane or polyethylene foam, or to non-woven textiles.Information provid..