Physical Properties Metric English Comments
Oxygen Transmission Rate 0.0931 cc/m²/day

@Temperature 23.0 °C
0.00600 cc/100 in²/day

@Temperature 73.4 °F
ExxonMobil Method
ExxonMobil Metallyte™ 28MWHB OPP Film
Product Description: A multi-layer, cavitaed, white OPP film that has exceptional barrier to gases, flavors and moistures. It is metalized on one side with a proprietary sealant layer on the other. ..
Oxygen Transmission Rate 0.0931 cc/m²/day
0.00600 cc/100 in²/day
ExxonMobil Method
ExxonMobil Metallyte™ 28UBW-ES OPP Film
Product Description: A multi-layer, cavitaed, white OPP film with an enhanced sealant to allow sealing through contamination. This film has an exceptional barrier to gases, flavors, and moisture. It..
Oxygen Transmission Rate 0.0931 cc/m²/day
0.00600 cc/100 in²/day
ExxonMobil Method
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film
Product Description: A multi-layer, cavitaed, white OPP film structure that has exceptional barrier to gases and flavors. It is metalized on one side and treated on the other. It is designed for use..
Oxygen Transmission Rate 0.0931 - 2100 cc/m²/day
0.00600 - 135 cc/100 in²/day
Average value: 375 cc/m²/day Grade Count:74
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..