Physical Properties Metric English Comments
Oxygen Transmission Rate 0.310 - 1.55 cc/m²/day
0.0200 - 0.0998 cc/100 in²/day
Average value: 1.08 cc/m²/day Grade Count:4
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..