Polymer Property : Oxygen Transmission Rate = 1.80 cc/100 in²/day
Polymer Property :
Oxygen Transmission Rate =
1.80 cc/100 in²/day
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Oxygen Transmission Rate
28.0
cc/m²/day
1.80
cc/100 in²/day
65% RH,23°C
UBE 5034C2 NCH Nylon 6/66 Film
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.