Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 10.0 cc/m²/day | 0.644 cc/100 in²/day | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Oxygen Transmission Rate | 10.0 cc/m²/day | 0.644 cc/100 in²/day | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |
|||
Oxygen Transmission Rate | 10.0 cc/m²/day | 0.644 cc/100 in²/day | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® G 16 PA6I/6T Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co.. |