Oxygen Transmission Rate 2.05 cc/m²/day
0.132 cc/100 in²/day
73°F (23°C) / 0%RH; ASTM D3985
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of ..