Oxygen Transmission Rate 210 cc/m²/day

@Thickness 1.80 mm,
Temperature 21.0 °C
13.5 cc/100 in²/day

@Thickness 0.0709 in,
Temperature 69.8 °F
ASTM D3985
PolyOne Versaflex™ HC MT226 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT226 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT226 has been specially formulated to be free of any plasticizers . ..