Physical Properties Metric English Comments
Oxygen Transmission Rate 5000 cc/m²/day
322 cc/100 in²/day
At 25°C/0% RH/1 bar; ASTM D3985
Borealis Borstar® FB2230 LLDPE for Film
Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..
Oxygen Transmission Rate 5000 cc/m²/day
322 cc/100 in²/day
At 25°C/0% RH/1 bar; ASTM D3985
Borealis Borstar® FB4230 LLDPE for Film
Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar ..