Physical Properties Metric English Comments
Oxygen Transmission Rate 20.18 - 35.7 cc/m²/day
1.300 - 2.30 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ 2500 Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr..
Oxygen Transmission Rate 18.62 - 35.7 cc/m²/day
1.199 - 2.30 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® Emblem™ 2500M M-Coated Bi-Axially Oriented Nylon Film
Description: Capran® Emblem™ 2500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd..