Polymer Property : Oxygen Transmission Rate = 406 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 2000 - 6300 cc/m²/day
129 - 406 cc/100 in²/day
Average value: 3980 cc/m²/day Grade Count:8
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..