Polymer Property : Oxygen Transmission Rate = 49.7 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 49.7 cc/m²/day

@Temperature 23.0 °C
3.20 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Metallyte™ 18MM488 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c..