Polymer Property : Oxygen Transmission Rate = 4900 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 4900 cc/m²/day
316 cc/100 in²/day
ASTM D3985
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film
This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac..