Physical Properties Metric English Comments
Oxygen Transmission Rate 751 cc/m²/day

@Temperature 23.0 °C
48.4 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MBT666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r..