Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.43 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.43 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SABIC P5510 Black High Density Polyethylene for Pipes Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |