Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.85 g/10 min @Load 21.6 kg, Temperature 190 °C |
0.85 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Melt Flow | 0.85 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.85 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Ineos TUB 172 HDPE TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T.. |
|||
Melt Flow | 0.85 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.85 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |