Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 190 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 374 °F |
ASTM D1238 |
Techmer ES Luriblend® PE 5903 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Melt Flow | 1.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
1.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Melt Flow | 1.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Melt Flow | 1.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 6501 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 7401 Injection Molding Grade, Extra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 7502 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |