Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.2 - 10.8 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.2 - 10.8 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6751E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 7.2 - 10.8 g/10 min @Load 21.6 kg, Temperature 190 °C |
7.2 - 10.8 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6752E (516H5) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |