Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 105 g/10 min @Load 2.16 kg, Temperature 180 °C |
105 g/10 min @Load 4.76 lb, Temperature 356 °F |
ASTM D1238 |